Title: Working Mechanism of Superplasticizer in Cement Paste with Fluoride Ion

Author(s): Kazuki Matsuzawa, Daiki Atarashi, Masahiro Miyauchi, Etsuo Sakai

Publication: JCI

Volume: 13

Issue: 6

Appears on pages(s): 305 - 310

Keywords:

DOI: 10.3151/jact.13.305

Date: 1/1/2015

Abstract: