Title: Influence of Fatigue Loading in Shear Failures of Reinforced Concrete Members without Transverse Reinforcement

Author(s): Miguel Fernández Ruiz, Carlos Zanuy, Francisco Natário, Juan Manuel Gallego, Luis Albajar, Aurelio Muttoni, Yuya Suda

Publication: JCI

Volume: 13

Issue: 5

Appears on pages(s): 263 - 274

Keywords:

DOI: 10.3151/jact.13.263

Date: 1/1/2015

Abstract:


Japan Concrete Institute, International Partner Access

View Resource »