Title: Corrosion of Steel Bars in Concrete with the Variation of Microstructure of Steel-Concrete Interface

Author(s): Tarek Uddin Mohammed, Hidenori Hamada, Ariful Hasnat, Mohammed Abdullah Al Mamun

Publication: JCI

Volume: 13

Issue: 4

Appears on pages(s): 230 - 240

Keywords:

DOI: 10.3151/jact.13.230

Date: 1/1/2015

Abstract: