Title: Flexural Behavior of Fire-Damaged Reinforced Concrete Slabs Repaired with Near-Surface Mounted (NSM) Carbon Fiber Reinforced Polymer (CFRP) Rods

Author(s): Cao Nguyen Thi, Withit Pansuk, Lluis Torres

Publication: JCI

Volume: 13

Issue: 1

Appears on pages(s): 15 - 29

Keywords:

DOI: 10.3151/jact.13.15

Date: 1/1/2015

Abstract: