Title: Chloride ingress in cracked concrete: a laser induced breakdown spectroscopy (LIBS) study

Author(s): Branko Šavija, Erik Schlangen, José Pacheco, Steven Millar, Thorsten Eichler, Gerd Wilsch

Publication: JCI

Volume: 12

Issue: 10

Appears on pages(s): 425 - 442

Keywords:

DOI: 10.3151/jact.12.425

Date: 1/1/2014