Title: Performance of Different Grades of Palm Oil Fuel Ash with Ground Slag as Base Materials in the Synthesis of Alkaline Activated Mortar

Author(s): Moruf Olalekan Yusuf, Megat Azmi Megat Johari, Zainal Arifin Ahmad, Mohammed Maslehuddin

Publication: JCI

Volume: 12

Issue: 10

Appears on pages(s): 378 - 387