International Concrete Abstracts Portal

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effective Recycling of Surface Modification Aggregate using Microwave Heating

Author(s): Heesup Choi, Ryoma Kitagaki, Takafumi Noguchi

Publication: JCI

Volume: 12

Issue: 2

Appears on pages(s): 34 - 45

Keywords:

DOI: 10.3151/jact.12.34

Date: 1/1/2014

Abstract:


Japan Concrete Institute, International Partner Access

View Resource »