Title: Assessment of Blended Cements Effectiveness Against ASR by Mortar and Concrete Expansion Tests

Author(s): Umberto Costa, Teresa Mangialardi, Antonio Evangelista Paolini

Publication: JCI

Volume: 12

Issue: 8

Appears on pages(s): 266 - 278

Keywords:

DOI: 10.3151/jact.12.266

Date: 1/1/2014

Abstract:


Japan Concrete Institute, International Partner Access