Title: Improving the Engineering and Fluid Transport Properties of Ultra-High Strength Concrete Utilizing Ultrafine Palm Oil Fuel Ash

Author(s): Ahmad N. Mohammed, Megat Azmi Megat Johari, Abdullah M. Zeyad, Bassam A. Tayeh, Moruf O. Yusuf

Publication: JCI

Volume: 12

Issue: 4

Appears on pages(s): 127 - 137

Keywords:

DOI: 10.3151/jact.12.127

Date: 1/1/2014