Title: Durability of Recycled Aggregate Concrete: An Overview

Author(s): Jianzhuang Xiao, Deng Lu, Jingwei Ying

Publication: JCI

Volume: 11

Issue: 12

Appears on pages(s): 347 - 359

Keywords:

DOI: 10.3151/jact.11.347

Date: 1/1/2013

Abstract: