Title: Kinematics on Split-Tensile Test of Fiber-Reinforced Concrete by AE

Author(s): Mielke R. I. A. J. Mondoringin, Masayasu Ohtsu

Publication: JCI

Volume: 11

Issue: 8

Appears on pages(s): 196 - 205

Keywords:

DOI: 10.3151/jact.11.196

Date: 1/1/2013