ACI Global Home Middle East Region Portal Western Europe Region Portal
Email Address is required Invalid Email Address
In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Topics In Concrete
Home > Publications > International Concrete Abstracts Portal
The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.
Title: Durability against Steel Corrosion of HPFRCC with Bending Cracks
Author(s): Shinichi Miyazato, Youichi Hiraishi
Publication: JCI
Volume: 11
Issue: 4
Appears on pages(s): 135 - 143
Keywords:
DOI: 10.3151/jact.11.135
Date: 1/1/2013
Abstract:
Japan Concrete Institute, International Partner Access
View Resource »