International Concrete Abstracts Portal

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Electro-Osmosis Applied for Formwork Removal of Concrete

Author(s): Nassima Goudjil, Yannick Vanhove, Chafika Djelal, Hassina Kada

Publication: JCI

Volume: 10

Issue: 9

Appears on pages(s): 301 - 312

Keywords:

DOI: 10.3151/jact.10.301

Date: 1/1/2012

Abstract:


Japan Concrete Institute, International Partner Access