International Concrete Abstracts Portal

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Hydration Kinetics of a Low Carbon Cementitious Material Produced by Physico-Chemical Activation of High Calcium Fly Ash

Author(s): Monower Sadique, Hassan Al-Nageim

Publication: JCI

Volume: 10

Issue: 8

Appears on pages(s): 254 - 263

Keywords:

DOI: 10.3151/jact.10.254

Date: 1/1/2012

Abstract:


Japan Concrete Institute, International Partner Access