International Concrete Abstracts Portal

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Investigation on Reaction Rate and Self-healing Ability in Fly Ash Blended Cement Mixtures

Author(s): Seung Hyun Na, Yukio Hama, Madoka Taniguchi, Osamu Katsura, Takahiro Sagawa, Mohamed Zakaria

Publication: JCI

Volume: 10

Issue: 7

Appears on pages(s): 240 - 253

Keywords:

DOI: 10.3151/jact.10.240

Date: 1/1/2012

Abstract:


Japan Concrete Institute, International Partner Access

View Resource »