Title: Reinforced Concrete Panels Subjected to Uniaxial and Biaxial Tension

Author(s): Nabil Dawood, Hesham Marzouk

Publication: JCI

Volume: 8

Issue: 1

Appears on pages(s): 59 - 73

Keywords:

DOI: 10.3151/jact.8.59

Date: 1/1/2010