Title: Influence of Patch Repair Material on Electrochemical Desalination of Concrete

Author(s): Hiroshi Minagawa, Makoto Hisada

Publication: JCI

Volume: 8

Issue: 3

Appears on pages(s): 281 - 290

Keywords:

DOI: 10.3151/jact.8.281

Date: 1/1/2010

Abstract:


Japan Concrete Institute, International Partner Access