International Concrete Abstracts Portal

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effects of Maintenance Strategies on the Life-cycle Performance and Cost of a Deteriorating RC Building with High-Seismic Hazard

Author(s): Chien-Kuo Chiu, Takafumi Noguchi, Manabu Kanematsu

Publication: JCI

Volume: 8

Issue: 2

Appears on pages(s): 157 - 170

Keywords:

DOI: 10.3151/jact.8.157

Date: 1/1/2010

Abstract:


Japan Concrete Institute, International Partner Access