Title: Tension Stiffening Model for Numerical Analysis of RC Structures by Using Bond-Slip Relationship

Author(s): Sam-Young Noh

Publication: JCI

Volume: 7

Issue: 1

Appears on pages(s): 61 - 78

Keywords:

DOI: 10.3151/jact.7.61

Date: 1/1/2009