Title: Modification of Test Process of PERMIT Ion Migration Test and its Application to Determinate Effect of Methods to Improve Chloride Penetration Resistance of Cover Concrete

Author(s): Jinbo Yang, Peiyu Yan

Publication: JCI

Volume: 7

Issue: 3

Appears on pages(s): 385 - 391

Keywords:

DOI: 10.3151/jact.7.385

Date: 1/1/2009

Abstract:


Japan Concrete Institute, International Partner Access