Title: Biaxial Fracture Behaviour of Steel-Span and Steel-Fibre- Reinforced Concrete

Author(s): Elmar K. Tschegg

Publication: JCI

Volume: 7

Issue: 2

Appears on pages(s): 229 - 238

Keywords:

DOI: 10.3151/jact.7.229

Date: 1/1/2009