Title: Self-Healing Capability of Fibre Reinforced Cementitious Composites

Author(s): Daisuke Homma, Hirozo Mihashi, Tomoya Nishiwaki

Publication: JCI

Volume: 7

Issue: 2

Appears on pages(s): 217 - 228

Keywords:

DOI: 10.3151/jact.7.217

Date: 1/1/2009

Abstract: