Title: Relation between the Shape of Silica Fume and the Fluidity of Cement Paste at Low Water to Powder Ratio

Author(s): Etsuo Sakai, Yasuo Kakinuma, Kenji Yamamoto, Masaki Daimon

Publication: JCI

Volume: 7

Issue: 1

Appears on pages(s): 13 - 20

Keywords:

DOI: 10.3151/jact.7.13

Date: 1/1/2009

Abstract: