Title: Effect of Aggregate on Drying Shrinkage of Concrete

Author(s): Tadashi Fujiwara

Publication: JCI

Volume: 6

Issue: 1

Appears on pages(s): 31 - 44

Keywords:

DOI: 10.3151/jact.6.31

Date: 1/1/2008

Abstract: