International Concrete Abstracts Portal

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Characterizing the 3D Pore Structure of Hardened Cement Paste with Synchrotron Microtomography

Author(s): Michael Angelo B. Promentilla, Takafumi Sugiyama, Takashi Hitomi, Nobufumi Takeda

Publication: JCI

Volume: 6

Issue: 2

Appears on pages(s): 273 - 286

Keywords:

DOI: 10.3151/jact.6.273

Date: 1/1/2008

Abstract:


Japan Concrete Institute, International Partner Access

View Resource »