International Concrete Abstracts Portal

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Comparative Tests of Beams and Columns Made of Recycled Aggregate Concrete and Natural Aggregate Concrete

Author(s): Andrzej B. Ajdukiewicz, Alina T. Kliszczewicz

Publication: JCI

Volume: 5

Issue: 2

Appears on pages(s): 259 - 273

Keywords:

DOI: 10.3151/jact.5.259

Date: 1/1/2007

Abstract:


Japan Concrete Institute, International Partner Access

View Resource »