Title: A Cohesive Interface Model for the Pullout of Inclined Steel Fibers in Cementitious Matrixes

Author(s): Alessandro P. Fantilli, Paolo Vallini

Publication: JCI

Volume: 5

Issue: 2

Appears on pages(s): 247 - 258

Keywords:

DOI: 10.3151/jact.5.247

Date: 1/1/2007