Title: Method of test for bending moment-curvature curve of fiber-reinforced cementitious composites

Author(s): Appendix

Publication: JCI

Volume: 4

Issue: 1

Appears on pages(s): 73 - 78

Keywords:

DOI: 10.3151/jact.4.73

Date: 1/1/2006

Abstract:


Japan Concrete Institute, International Partner Access