Title: Estimation of Chloride Diffusion Coefficent of Concrete Using Mineral Admixtures

Author(s): Tatsuhiko Saeki, Kenji Sasaki, Kenta Shinada

Publication: JCI

Volume: 4

Issue: 3

Appears on pages(s): 385 - 394

Keywords:

DOI: 10.3151/jact.4.385

Date: 1/1/2006

Abstract:


Japan Concrete Institute, International Partner Access