Title: Nondestructive Evaluation of Damaged Concrete due to Freezing and Thawing by Elastic-Wave Method

Author(s): Masayasu Ohtsu

Publication: JCI

Volume: 3

Issue: 3

Appears on pages(s): 333 - 341

Keywords:

DOI: 10.3151/jact.3.333

Date: 1/1/2005

Abstract:


Japan Concrete Institute, International Partner Access