Title: Evaluation of Ultimate Strength of Post-Tensioned Anchorage Zones

Author(s): Young Mook Yun

Publication: JCI

Volume: 3

Issue: 1

Appears on pages(s): 149 - 159

Keywords:

DOI: 10.3151/jact.3.149

Date: 1/1/2005

Abstract:


Japan Concrete Institute, International Partner Access

View Resource »