Title: Analysis of FRP-Strengthened RC Members with Varied Sheet Bond Stress-Slip Models

Author(s): HuneBum Ko, Yuichi Sato

Publication: JCI

Volume: 2

Issue: 3

Appears on pages(s): 317 - 326

Keywords:

DOI: 10.3151/jact.2.317

Date: 1/1/2004