Title: Snapback Failure Analysis for Large Scale Concrete Structures and its Application to Shear Capacity Study of Columns

Author(s): Tada-aki Tanabe, Atsushi Itoh, Naoshi Ueda

Publication: JCI

Volume: 2

Issue: 3

Appears on pages(s): 275 - 288

Keywords:

DOI: 10.3151/jact.2.275

Date: 1/1/2004

Abstract:


Japan Concrete Institute, International Partner Access