International Concrete Abstracts Portal

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Study on the Properties of High Strength Concrete using High Belite Cement

Author(s): Tongbo Sui, Lei Fan, Zhaijun Wen, Jing Wang, Zhonglun Zhang

Publication: JCI

Volume: 2

Issue: 2

Appears on pages(s): 201 - 206

Keywords:

DOI: 10.3151/jact.2.201

Date: 1/1/2004

Abstract:


Japan Concrete Institute, International Partner Access