International Concrete Abstracts Portal

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Numerical Modeling of Steel Corrosion in Concrete Structures due to Chloride Ion, Oxygen and Water Movement

Author(s): Tsuyoshi Maruya, Kailin Hsu, Hitoshi Takeda, Somnuk Tangtermsirikul

Publication: JCI

Volume: 1

Issue: 2

Appears on pages(s): 147 - 160

Keywords:

DOI: 10.3151/jact.1.147

Date: 1/1/2003

Abstract:


Japan Concrete Institute, International Partner Access

View Resource »