Title: Hot Weather Concreting in South Louisiana

Author(s): TJ Harris

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 11/14/2017

Abstract:
Contractors, Specifiers, Concrete Producers and Concrete Testing Agencies will be able to better understand the impact of time, temperature and drum revolutions on the performance of ready-mix concrete during production and placement of concrete during hot weather.