Evaluating Structural Buildup at Rest of Self-Consolidating Concrete Using Workability Tests

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Evaluating Structural Buildup at Rest of Self-Consolidating Concrete Using Workability Tests

Author(s): Wael A. Megid and Kamal H. Khayat

Publication: Materials Journal

Volume: 115

Issue: 2

Appears on pages(s): 257-265

Keywords: rheology; self-consolidating concrete; static yield stress; structural buildup; thixotropy; workability loss

DOI: 10.14359/51701240

Date: 3/1/2018

Abstract:
Structural buildup at rest (SBR) is a rheological property that can affect the performance of self-consolidating concrete (SCC). Such a property should be optimized to intended placement condition. Adequate determination of SBR on the jobsite is important for quality control, thus necessitating the use of simple and robust testing methods. The ability of employing conventional workability test methods to evaluate SBR of SCC is discussed. Eight SCC mixtures designed to secure different SBR levels were investigated. SBR was determined using concrete rheometer and two field-oriented test methods: portable vane and inclined plane, as well as losses of slump flow, T50, and J-ring flow at rest. Correlations between SBR indexes determined from workability and rheological test methods were established. Statistical models to predict static yield stress and SBR indexes as a function of workability loss at rest are proposed, which indicate that standard workability test methods can be used to evaluate SBR of SCC.

Related References:

1. Tattersall, G., Workability and Quality Control of Concrete, E&FN Spon, London, UK, 1991, 262 pp.

2. Tattersall, G., and Banfill, P., The Rheology of Fresh Concrete, Pitman Advanced Publishing, Boston, MA, 1983, 368 pp.

3. Khayat, K., and Mitchell, D., “Self-Consolidating Concrete for Precast, Prestressed Concrete Bridge Elements,” National Cooperative Highway Research Program (NCHRP) Report 628, Transportation Research Board, Washington, DC, 2009, 91 pp.

4. Khayat, K., and Omran, A., “Evaluation of SCC Formwork Pressure,” Concrete in Focus, July-Aug. 2009, pp. 16-21.

5. Tattersall, G. H., and Bloomer, S. J., “Further Development of the Two-Point Test for Workability and Extension of Its Range,” Magazine of Concrete Research, V. 31, No. 109, 1979, pp. 202-210. doi: 10.1680/macr.1979.31.109.202

6. Tattersall, G., “Relationship between the British Standard Tests for Workability and the Two-Point Test,” Magazine of Concrete Research, V. 28, No. 96, 1976, pp. 143-147. doi: 10.1680/macr.1976.28.96.143

7. Scullion, T., “The Measurement of the Workability of Fresh Concrete,” M.Sc(Eng) dissertation, University of Sheffield, Sheffield, UK, 1975.

8. Morinaga, M., “Pumpability of Concrete and Pumping Pressure in Pipelines, Fresh Concrete: Important Properties and Their Measurement,” Proceedings of a RILEM Conference, Leeds, England, V. 7, Mar. 1973, pp. 7.3-1 to 7.3-39.

9. Murata, J., “Flow and Deformation of Fresh Concrete,” Materials and Structures, V. 17, No. 98, 1984, pp. 117-129.

10. Christensen, G., “Modeling the Flow Properties of Fresh Concrete: The Slump Test,” PhD thesis, Princeton University, Princeton, NJ, 1991, 22 pp.

11. Schowalter, W., and Christensen, G., “Toward a Rationalization of the Slump Test for Fresh Concrete: Comparisons of Calculations and Experiments,” Journal of Rheology (New York, N.Y.), V. 42, No. 4, 1998, pp. 865-870. doi: 10.1122/1.550905

12. Clayton, S.; Grice, T.; and Boger, D., “Analysis of the Slump Test for On-Site Yield Stress Measurement of Mineral Suspensions,” International Journal of Mineral Processing, V. 70, No. 1-4, 2003, pp. 3-21. doi: 10.1016/S0301-7516(02)00148-5

13. Hu, C.; de Larrard, F.; Sedran, T.; Boulay, C.; Bosc, F.; and Deflorenne, F., “Validation of BTRHEOM, the New Rheometer for Soft-to-Fluid Concrete,” Materials and Structures, V. 29, No. 10, 1996, pp. 620-631. doi: 10.1007/BF02485970

14. Roussel, N., “Correlation between Yield Stress and Slump: Comparison between Numerical Simulations and Concrete Rheometers Results,” Materials and Structures, V. 39, No. 4, 2007, pp. 501-509. doi: 10.1617/s11527-005-9035-2

15. Saak, A.; Jennings, H.; and Shah, S., “A Generalized Approach for the Determination of Yield Stress by Slump and Slump Flow,” Cement and Concrete Research, V. 34, No. 3, 2004, pp. 363-371. doi: 10.1016/j.cemconres.2003.08.005

16. Hu, C., and de Larrard, F., “The Rheology of Fresh High-Performance Concrete,” Cement and Concrete Research, V. 26, No. 2, 1996, pp. 283-294. doi: 10.1016/0008-8846(95)00213-8

17. Barnes, H., “Thixotropy—A Review,” Journal of Non-Newtonian Fluid Mechanics, V. 70, No. 1-2, 1997, pp. 1-33. doi: 10.1016/S0377-0257(97)00004-9

18. Khayat, K.; Omran, A.; and Megid, W., “Evaluation of Thixotropy of Self-Consolidating Concrete and Influence on Concrete Performance,” ANAIS Do 54º Congresso Brasileiro Do Concreto CBC2012–54CBC, Maceió, Alagoas, Brazil, Oct. 2012, 14 pp.

19. ACI Committee 238, “Concrete Thixotropy (ACI 238.2T-14),” American Concrete Institute, Farmington Hills, MI, 2014, 6 pp.

20. Billberg, P., “Development of SCC Static Yield Stress at Rest and Its Effect on the Lateral Form Pressure,” SCC 2005: Proceedings of 2nd North American Conference on the Design and Use of Self-Consolidating Concrete and 4th International RILEM Symposium on Self-Compacting Concrete, Chicago, 2005, pp. 583-589.

21. Ovarlez, G., and Roussel, N., “A Physical Model for the Prediction of Lateral Stress Exerted by Self-Compacting Concrete on Formwork,” Materials and Structures, V. 37, No. 2, 2006, pp. 239-248.

22. Megid, W., and Khayat, K., “Bond Strength in Multilayer Castings of Self-Consolidating Concrete,” ACI Materials Journal, V. 114, No. 3, May-June 2017, pp. 467-476. doi: 10.14359/51689597

23. Roussel, N., and Cussigh, F., “Distinct-Layer Casting of SCC: The Mechanical Consequences of Thixotropy,” Cement and Concrete Research, V. 38, No. 5, 2008, pp. 624-632. doi: 10.1016/j.cemconres.2007.09.023

24. Khayat, K., and Omran, A., “Evaluation of SCC Formwork Pressure,” Second International Symposium on Design, Performance and Use of Self-Consolidating Concrete, Beijing, China, 2009, pp. 43-55.

25. Assaad, J.; Khayat, K.; and Mesbah, H., “Assessment of Thixotropy of Flowable and Self-Consolidating Concrete,” ACI Materials Journal, V. 100, No. 2, Mar.-Apr. 2003, pp. 99-107.

26. Omran, A.; Naji, S.; and Khayat, K., “Portable Vane Test to Assess Structural Build-Up at Rest of Self-Consolidating Concrete,” ACI Materials Journal, V. 108, No. 6, Nov.-Dec. 2011, pp. 628-637.

27. Coussot, P., and Boyer, S., “Determination of Yield Stress Fluid Behavior from Inclined Plane Test,” Rheologica Acta, V. 34, No. 6, 1995, pp. 534-543. doi: 10.1007/BF00712314

28. CAN/CSA-A3000-13, “Cementitious Materials Compendium,” CSA Group, Toronto, ON, Canada, 2003, 308 pp.

29. ASTM C1157-02, “Standard Performance Specification for Hydraulic Cement,” ASTM International, West Conshohocken, PA, 2002, 6 pp.

30. CSA A23.1-14/A23.2-14, “Concrete Materials and Methods of Concrete Construction/Test Methods and Standard Practices for Concrete,” CSA Group, Toronto, ON, Canada, 2014, 690 pp.

31. Khayat, K., and Yahia, A., “Modification of the Concrete Rheometer to Determine Rheological Parameters of Self-Consolidating Concrete-Vane Device,” Proceedings of the 2nd International RILEM Symposium on Advances in Concrete through Science and Engineering, J. Marchand et al., eds., Québec City, QC, Canada, 2006, pp. 375-380.

32. Dzuy, Q., and Boger, V., “Direct Yield Stress Measurement with the Vane Method,” Journal of Rheology (New York, N.Y.), V. 29, No. 3, 1985, pp. 335-347. doi: 10.1122/1.549794

33. Khayat, K.; Omran, A.; and Pavate, T., “Inclined Plane Test Method to Determine Structural Build-Up at Rest of Self-Consolidating Concrete,” ACI Materials Journal, V. 107, No. 5, Sept.-Oct. 2010, pp. 515-522.

34. Oremus, R., “A One-Dimensional Model of Dense Snow Avalanches Using Mass and Momentum Balances,” MSc thesis, Humboldt State University, Arcata, CA, 2006, 71 pp.

35. ASTM C1611/C1611M-14, “Standard Test Method for Slump Flow of Self-Consolidating Concrete,” ASTM International, West Conshohocken, PA, 2014, 6 pp.

36. ASTM C1621/1621M-17, “Standard Test Method for Passing Ability of Self-Consolidating Concrete by J-Ring,” ASTM International, West Conshohocken, PA, 2017, 4 pp.

37. EFNARC, “Specification and Guidelines for Self-Compacting Concrete,” European Federation of National Associations Representing for Concrete, Feb. 2002, p. 22.

38. Bosiljkov, V. B., “Experience with Self-Compacting Concrete Made from Local Materials,” Innovation and Developments in Concrete Materials and Construction, Proceedings of International Conference, University of Dundee, Scotland, UK, Sept. 2002, pp. 423-432.

39. Khayat, K.; Omran, A.; Naji, S.; Billberg, P.; and Yahia, A., “Field-Oriented Test Methods to Evaluate Structural Build-Up at Rest of Flowable Mortar and Concrete,” Materials and Structures, V. 45, No. 10, 2012, pp. 1547-1564. doi: 10.1617/s11527-012-9856-8


ALSO AVAILABLE IN:

Electronic Materials Journal