Mechanical and Durability Properties of Concrete Produced with Treated Recycled Concrete Aggregate

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Mechanical and Durability Properties of Concrete Produced with Treated Recycled Concrete Aggregate

Author(s): V. Bhasya and B. H. Bharatkumar

Publication: Materials Journal

Volume: 115

Issue: 2

Appears on pages(s): 209-217

Keywords: durability; mechanical properties; mineral admixtures; sustainable concrete; treated recycled concrete aggregate

DOI: 10.14359/51701239

Date: 3/1/2018

Abstract:
The presence of attached mortar is the main reason for lower quality of recycled concrete aggregate (RCA) compared to that of natural aggregate. Hence, its use is limited up to 30% replacement of natural aggregate at present. The attached mortar of the RCA can be removed by mechanical treatment, acid treatment, thermal treatment (500 to 750°C [932 to 1382°F]), and microwave treatment. There are difficulties—such as achieving high temperature and treating larger quantities of RCA with acid and a microwave oven—in applying these treatments at field level. Hence, the present study focuses on a combination of heating (250°C [482°F]) and mechanical treatment to improve the quality of the RCA. This method removed 70 to 80% of attached mortar of the RCA. Properties of RCA such as bulk density, specific gravity, water absorption, and crushing value were discussed in detail. Post-treatment, it was observed that the properties of treated RCA improved compared to untreated RCA, but still they were found to be poorer than natural aggregate. The experimental studies were carried out to overcome the aforementioned drawbacks of the recycled aggregate concrete by incorporation of mineral admixtures. It was found that the use of mineral admixtures in concrete produced with treated RCA enhances both the mechanical and durability properties. Thus, the concrete produced with treated RCA and mineral admixture will lead to sustainable development.

Related References:

1. Rao, A.; Jha, K. N.; and Misra, S., “Use of Aggregates from Recycled Construction and Demolition Waste in Concrete,” Resources, Conservation and Recycling, V. 50, No. 1, 2007, pp. 71-81. doi: 10.1016/j.resconrec.2006.05.010

2. Bhashya, V., and Bharatkumar, B. H., “Effect of Different Sources and Crushing Type on the Properties of Recycled Aggregate Concrete,” Proceedings of the International Conference on Sustainable Energy and Built Environment, ASCE India Section-VIT University, Vellore, India, Mar. 2015, pp. 953-956.

3. Rao, M. C.; Bhattacharyya, S. K.; and Barai, S. V., “Recycled Coarse Aggregate and Its Use in Concrete,” Indian Concrete Institute Journal, V. 11, No. 4, 2011, pp. 27-40.

4. Meyer, C., “The Greening of the Concrete Industry,” Cement and Concrete Composites, V. 31, No. 8, 2009, pp. 601-605. doi: 10.1016/j.cemconcomp.2008.12.010

5. Yuan, F.; Shen, L. Y.; and Li, Q. M., “Energy Analysis of the Recycling Options for Construction and Demolition Waste,” Waste Management (New York, N.Y.), V. 31, No. 12, 2011, pp. 2503-2511. doi: 10.1016/j.wasman.2011.07.001

6. Yu, A. T.; Poon, C. S.; Wong, A.; Yip, R.; and Jaillon, L., “Impact of Construction Waste Disposal Charging Scheme on Work Practices at Construction Sites in Hong Kong,” Waste Management (New York, N.Y.), V. 33, No. 1, 2013, pp. 138-146. doi: 10.1016/j.wasman.2012.09.023

7. Rao, M. C.; Bhattacharyya, S. K.; and Barai, S. V., “Behaviour of Recycled Aggregate Concrete under Drop Weight Impact Load,” Construction and Building Materials, V. 25, No. 1, 2011, pp. 69-80. doi: 10.1016/j.conbuildmat.2010.06.055

8. Belén, G. F.; Fernando, M. A.; Diego, C. L.; and Sindy, S. P., “Stress-Strain Relationship in Axial Compression for Concrete Using Recycled Saturated Coarse Aggregate,” Construction and Building Materials, V. 25, No. 5, 2011, pp. 2335-2342. doi: 10.1016/j.conbuildmat.2010.11.031

9. Grabiec, A. M.; Klama, J.; Zawal, D.; and Krupa, D., “Modification of Recycled Concrete Aggregate by Calcium Carbonate Bio Deposition,” Construction and Building Materials, V. 34, 2012, pp. 145-150. doi: 10.1016/j.conbuildmat.2012.02.027

10. Tam, V. W.; Tam, C. M.; and Le, K. N., “Removal of Cement Mortar Remains from Recycled Aggregate Using Pre-soaking Approaches,” Resources, Conservation and Recycling, V. 50, No. 1, 2007, pp. 82-101. doi: 10.1016/j.resconrec.2006.05.012

11. Akbarnezhad, A.; Ong, K. C. G.; Zhang, M. H.; Tam, C. T.; and Foo, T. W. J., “Microwave-Assisted Beneficiation of Recycled Concrete Aggregates,” Construction and Building Materials, V. 25, No. 8, 2011, pp. 3469-3479. doi: 10.1016/j.conbuildmat.2011.03.038

12. Naguchi, T., “Sustainable Recycling of Concrete Structures,” Indian Concrete Institute Journal, V. 13, No. 1, Apr.-June 2012, pp. 41-53.

13. Revathi, P., and Sasikala, M., “Studies on Fresh and Hardened Properties of Recycled Aggregate Concrete with Quarry Dust,” ACI Materials Journal, V. 111, No. 3, May-June 2014, pp. 283-290.

14. de Juan, M. S., and Gutiérrez, P. A., “Study on the Influence of Attached Mortar Content on the Properties of Recycled Concrete Aggregate,” Construction and Building Materials, V. 23, No. 2, 2009, pp. 872-877. doi: 10.1016/j.conbuildmat.2008.04.012

15. Al-Bayati, H. K. A.; Das, P. K.; Tighe, S. L.; and Baaj, H., “Evaluation of Various Treatment Methods for Enhancing the Physical and Morphological Properties of Coarse Recycled Concrete Aggregate,” Construction and Building Materials, V. 112, 2016, pp. 284-298. doi: 10.1016/j.conbuildmat.2016.02.176

16. IS 12269-1987, “Specifications for 53 Grade Ordinary Portland Cement,” Bureau of Indian Standards, New Delhi, India, 1987, pp. 1-5.

17. IS 4031-1988, “Methods of Physical Tests for Hydraulic Cement,” Bureau of Indian Standards, New Delhi, India, 1988, pp. 1-5.

18. IS 1727-1967, “Methods of Test for Pozzolanic Materials,” Bureau of Indian Standards, New Delhi, India, 1967, pp. 13-21.

19. Kim, K. H., and Cho, H. C., “Breakage of Waste Concrete by Free Fall,” Powder Technology, V. 200, No. 3, 2010, pp. 97-104. doi: 10.1016/j.powtec.2010.02.008

20. IS 10262-2009, “Concrete Mix Proportioning—Guidelines,” Bureau of Indian Standards, New Delhi, India, 2009, pp. 1-11.

21. ASTM C642-13, “Standard Test Method for Density, Absorption and Voids in Hardened Concrete,” ASTM International, West Conshohocken, PA, 2013, 3 pp.

22. ASTM C1202-12, “Standard Test Method for Electrical Indication of Concrete’s Ability to Resist Chloride Ion Penetration,” ASTM International, West Conshohocken, PA, 2012, 7 pp.

23. IS 2386-1963, “Methods of Test for Aggregates for Concrete,” Bureau of Indian Standards, New Delhi, India, 1963, pp. 3-8.

24. Somna, R.; Jaturapitakkul, C.; Chalee, W.; and Rattanachu, P., “Effect of the Water to Binder Ratio and Ground Fly Ash on Properties of Recycled Aggregate Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 24, No. 1, 2012, pp. 16-22. doi: 10.1061/(ASCE)MT.1943-5533.0000360

25. Shayan, A., and Xu, A., “Performance and Properties of Structural Concrete Made with Recycled Concrete Aggregate,” ACI Materials Journal, V. 100, No. 5, Sept.-Oct. 2003, pp. 371-380.

26. Quan, H.; Kasami, H.; and Tamai, T., “Experimental Study on Effects of Adhered Mortar Content on Quality of Recycled Coarse Aggregate and Properties of Concrete,” Second International Conference on Waste Engineering and Management, RILEM Publications, Paris, France, 2010, pp. 491-500.

27. Levy, S. M., and Helene, P., “Durability of Recycled Aggregates Concrete: A Safe Way to Sustainable Development,” Cement and Concrete Research, V. 34, No. 11, 2004, pp. 1975-1980. doi: 10.1016/j.cemconres.2004.02.009

28. Poon, C. S.; Shui, Z. H.; and Lam, L., “Effect of Microstructure of ITZ on Compressive Strength of Concrete Prepared with Recycled Aggregates,” Construction and Building Materials, V. 18, No. 6, 2004, pp. 461-468. doi: 10.1016/j.conbuildmat.2004.03.005

29. Tangchirapat, W.; Buranasing, R.; Jaturapitakkul, C.; and Chindaprasirt, P., “Influence of Rice Husk–Bark Ash on Mechanical Properties of Concrete Containing High Amount of Recycled Aggregates,” Construction and Building Materials, V. 22, No. 8, 2008, pp. 1812-1819. doi: 10.1016/j.conbuildmat.2007.05.004

30. Shima, H.; Tateyashiki, H.; Matsuhashi, R.; and Yoshida, Y., “An Advanced Concrete Recycling Technology and its Applicability Assessment through Input-Output Analysis,” Journal of Advanced Concrete Technology, V. 3, No. 1, 2005, pp. 53-67. doi: 10.3151/jact.3.53

31. Sui, Y., and Mueller, A., “Development of Thermo-Mechanical Treatment for Recycling of Used Concrete,” Materials and Structures, V. 45, No. 10, 2012, pp. 1487-1495. doi: 10.1617/s11527-012-9852-z

32. Wong, Y. D.; Sun, D. D.; and Lai, D., “Value Added Utilization of Recycled Concrete in Hot-Mix Asphalt,” Waste Management (New York, N.Y.), V. 27, No. 2, 2007, pp. 294-301. doi: 10.1016/j.wasman.2006.02.001

33. Pandurangan, K.; Dayanithy, A.; and Prakash, S. O., “Influence of Treatment Methods on the Bond Strength of Recycled Aggregate Concrete,” Construction and Building Materials, V. 120, 2016, pp. 212-221. doi: 10.1016/j.conbuildmat.2016.05.093

34. Revathi, P.; Ramesh, R.; and Lavanya, K., “Influence of Treatment Methods on the Strength and Performance Characteristics of Recycled Aggregate Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 27, No. 5, 2015, pp. 1-7. doi: 10.1061/(ASCE)MT.1943-5533.0001128

35. Ann, K. Y.; Moon, H. Y.; Kim, Y. B.; and Ryou, J., “Durability of Recycled Aggregate Concrete using Pozzolanic Materials,” Waste Management, V. 28, No. 6, 2008, pp. 993-999.

36. Katz, A., “Treatments for the Improvement of Recycled Aggregate,” Journal of Materials in Civil Engineering, ASCE, V. 16, No. 6, 2004, pp. 597-603. doi: 10.1061/(ASCE)0899-1561(2004)16:6(597)

37. Goldman, A., and Bentur, A., “The Influence of Microfillers on Enhancement of Concrete Strength,” Cement and Concrete Research, V. 23, No. 4, 1993, pp. 962-972.

38. Gonzalez-Corominas, A.; Etxeberria, M.; and Poon, C. S, “Influence of Steam Curing on the Pore Structures and Mechanical Properties of Fly Ash High Performance Concrete Prepared with Recycled Aggregates,” Cement and Concrete Composites, V. 71, 2016, pp. 77-84. doi: 10.1016/j.cemconcomp.2016.05.010

39. Lydon, F. D., and Balendran, R. V., “Some Observations on Elastic Properties of Plain Concrete,” Cement and Concrete Research, V. 16, No. 3, 1986, pp. 314-324. doi: 10.1016/0008-8846(86)90106-7

40. Eguchi, K.; Teranishi, K.; Nakagome, A.; Kishimoto, H.; Shinozaki, K.; and Narikawa, M., “Application of Recycled Coarse Aggregate by Mixture to Concrete Construction,” Construction and Building Materials, V. 21, No. 7, 2007, pp. 1542-1551. doi: 10.1016/j.conbuildmat.2005.12.023

41. de Brito, J. D., and Fatima, A., “Concrete with Recycled Aggregates: The Portuguese Experimental Research,” Materials and Structures, V. 43, 2010, pp. 35-51. doi: 10.1617/s11527-010-9595-7

42. Kou, S. C.; Poon, C. S.; and Chan, D., “Influence of Fly Ash as Cement Replacement on the Properties of Recycled Aggregate Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 19, No. 9, 2007, pp. 709-717. doi: 10.1061/(ASCE)0899-1561(2007)19:9(709)

43. Corinaldesi, V., and Moriconi, G., “Admixtures on Performance and Economics of Recycled Aggregate Concrete,” Seventh CANMET/ACI International Conference on Fly Ash, Silica Fume, Slag and Natural Pozzolans in Concrete, SP-199, V. M. Malhotra, ed., American Concrete Institute, Farmington Hills, MI, 2001, pp. 869-884.

44. Tazawa, E., “Engineering Scheme to Expedite Effective Use of Resources,” Proceedings of the International Symposium on Concrete Technology for Sustainable Development in the Twenty-First Century, Radha Press, New Delhi, India, 1999, pp. 23-42.


ALSO AVAILABLE IN:

Electronic Materials Journal