Title: ASR Damage Detection and Assessment of Supplementary Cementitious Materials Subjected to Environmental Loadings

Author(s): Shuaicheng Guo

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 10/24/2017

Abstract:
The special sessions will emphasize the durability of concrete bridges and buildings subjected to aggressive environmental or physical distress. Presentations will encompass a variety of technical aspects, such as the residual behavior of concrete members, performance of concrete structures reinforced or strengthened with fiber-reinforced polymer composites, and damage detection and assessment techniques. Both experimental and analytical investigations are of interest. The session brings to light recent research findings and provides an opportunity to discuss present challenges and technical demands. Critical information is given to those who lead tomorrow’s structural design and construction, including practicing engineers, government officials, and academics.