Experimental Study on Correlation between Resistivity Measurement Methods in Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Study on Correlation between Resistivity Measurement Methods in Concrete

Author(s): Hassan Parsian, Mohsen Tadayon, Davood Mostofinejad, and Farhad Avatefi

Publication: Materials Journal

Volume: 115

Issue: 1

Appears on pages(s): 33-45

Keywords: ASTM C1760; correlation; electrical resistivity; four-probe; impedance spectroscopy; one-probe

DOI: 10.14359/51701125

Date: 1/1/2018

Abstract:
The current research goal is to develop appropriate relationships to predict results of resistivity measurements of the standard ASTM C1760 test method using test data from some other methods: impedance spectroscopy, and one-probe and four-probe methods. For this purpose, 49 concrete mixtures with a vast variety of resistivity were tested under similar conditions. The one-probe method test specimens were rectangular slabs with an edge of 300 mm (12 in.) and a height of 110 mm (4.5 in.), and the other test specimens were 100 mm (4 in.) diameter cylinders with a 200 mm (8 in.) height. The outcomes demonstrated little difference between the results of impedance spectroscopy, and one-probe and modified four-probe methods with ASTM C1760 methods. The cell constant of one-probe method, based on standard method results, has been included into the calculation in a special condition. Some relations were also derived to predict the standard method results using the other method’s results.

Related References:

1. Whiting, D. A., and Nagi, M. A., “Electrical Resistivity of Concrete—Literature Review,” PCA R&D Serial No. 2457, Portland Cement Association, Skokie, IL, 2003, 57 pp.

2. Esbach, O. E., and Souders, M., Handbook of Engineering Fundamentals, John Wiley & Sons, Inc., New York, 1975, 1562 pp.

3. Harper, C. A., “Fundamentals of Electrical Insulating Materials,” Industrial Research/Development, V. 20, No. 12, 1978, pp. 81-84.

4. ASTM C876-91, “Standard Test Method for Half-Cell Potentials of Uncoated Reinforcing Steel in Concrete,” ASTM International, West Conshohocken, PA, 1991, 6 pp.

5. Polder, R.; Andrade, C.; Elsener, B.; Vennesland, Ø.; Gulikers, J.; Weidert, R.; and Raupach, M., “Test Methods for On Site Measurement of Resistivity of Concrete,” Materials and Structures, V. 33, No. 10, 2000, pp. 603-611. doi: 10.1007/BF02480599

6. Rajabipour, F., “Fundamental Investigations on Utilizing Electrical Sensing to Improve Life Cycle Modeling of Concrete Structures,” MSc thesis, Purdue University, West Lafayette, IN, 2003, 105 pp.

7. Andrade, C.; d’Andrea, R.; and Rebolledo, N., “Chloride Ion Penetration in Concrete: the Reaction Factor in the Electrical Resistivity Model,” Cement and Concrete Composites, V. 47, 2014, pp. 41-46. doi: 10.1016/j.cemconcomp.2013.09.022

8. Li, Z.; Xiao, L.; Wei, X.; and Zhang, J., “Interpretation of Microstructure Development of Cementitious Materials In Early Ages with Electrical Resistivity Measurement,” First International Conference on Microstructure Related Durability of Cementitious Composites, Nanjing, China, 2008, pp. 253-262.

9. Mei, Z. H., and Chung, D. D. L., “Effects of Temperature and Stress on the Interface between Concrete and Its Carbon Fiber Epoxy-Matrix Composite Retrofit, Studied by Electrical Resistance Measurement,” Cement and Concrete Research, V. 30, No. 5, 2000, pp. 799-802. doi: 10.1016/S0008-8846(00)00238-6

10. Gjorv, O. E.; Vennesland, O.; and El-Busaidy, A. H. S., “Electrical Resistivity of Concrete in the Oceans,” 9th Annual Offshore Technology Conference, Houston, TX, 1977, 8 pp.

11. Tuutti, K., Corrosion of Steel in Concrete, CBI, Stockholm, Sweden, 1982, pp. 78-81.

12. ASTM C1760-12, “Standard Test Method for Bulk Electrical Conductivity of Hardened Concrete,” ASTM International, West Conshohocken, PA, 2012, 5 pp.

13. Li, Z., and Li, W., “Contactless Transformer-Based Measurement of the Resistivity of Materials,” United States Patent No. Us 6, 639, 401 B2, 2003.

14. Elkey, W., and Sellevold, E.J., “Electrical Resistivity of Concrete,” Norwegian Road Research Laboratory, Publication No. 80, 1995, 36 pp.

15. Hammond, E., and Robson, T. D., “Comparison of Electrical Properties of Various Cements and Concretes,” The Engineer (London), V. 199, No. 5156, 1955, pp. 78-80.

16. Broomfield, J. B., Corrosion of Steel in Concrete, E&FN Spon, an Imprint of Chapman & Hall, London, UK, 1977, 238 pp.

17. Feliu, S.; Andrade, C.; González, J. A.; and Alonso, C., “A New Method for In-Situ Measurement of Electrical Resistivity of Reinforced Concrete,” Materials and Structures, V. 29, No. 6, 1996, pp. 362-365. doi: 10.1007/BF02486344

18. Elsener, B.; Fluckiger, D.; Wojtas, H.; and Bohni, H., “Methods for the Evaluation of Corrosion of Steel in Concrete,” VSS Report 521, Swiss Federal Department of Traffic and Energy, ASB Research for the Maintenance of Bridges, 1996, 140 pp.

19. Wenner, F., “A Method of Measuring Earth Resistivity,” Bulletin of the Bureau of Standards, V. 12, No. 4, 1916, pp. 469-478. doi: 10.6028/bulletin.282

20. Stratfull, R. F., “How Chlorides Affect Concrete Used with Reinforcing Steel,” Materials Protection, V. 7, No. 3, 1968, pp. 29-34.

21. Naish, C.C.; Harker, A.; and Carney, R.F.A., “Concrete Inspection: Interpretation of Potential and Resistivity Measurements,” 3rd International Symposium on Corrosion of Reinforcement in Concrete Construction, 1990, pp. 314-332.

22. Gowers, K. R., and Millard, S. G., “Measurement of Concrete Resistivity for Assessment of Corrosion Severity of Steel Using Wenner Technique,” ACI Materials Journal, V. 96, No. 5, Sept.-Oct. 1999, pp. 536-542.

23. Gowers, K. R., and Millard, S. G., “The Effect of Steel Reinforcement Bars on the Measurement of Concrete Resistivity,” British Journal of Non-Destructive Testing, V. 33, No. 11, 1991, pp. 551-554.

24. McCarter, W. J., and Barclay, S., “A Comparison of Two Methods for Resistivity Measurements on Repair Mortar for Cathodic Protection Systems,” Cement and Concrete Research, V. 23, No. 5, 1993, pp. 1178-1184. doi: 10.1016/0008-8846(93)90178-C

25. ASTM C127-01, “Standard Test Method for Relative Density (Specific Gravity) and Absorption of Coarse Aggregate,” ASTM International, West Conshohocken, PA, 2001, 6 pp.

26. ASTM C128-01, “Standard Test Method for Relative Density (Specific Gravity) and Absorption of Fine Aggregate,” ASTM International, West Conshohocken, PA, 2001, 6 pp.

27. ASTM C192-02, “Standard Test Method for Making and Curing Concrete Test Specimens in the Laboratory,” ASTM International, West Conshohocken, PA, 2002, 8 pp.

28. Morris, W.; Moreno, E. I.; and Sagües, A. A., “Practical Evaluation of Resistivity of Concrete in Test Cylinders Using a Wenner Array Probe,” Cement and Concrete Research, V. 26, No. 12, 1996, pp. 1779-1787. doi: 10.1016/S0008-8846(96)00175-5


ALSO AVAILABLE IN:

Electronic Materials Journal