Abstract:
Full-scale reinforced concrete (RC) and ultra-high-performance fiber-reinforced concrete (UHP-FRC) columns subjected to reversed cyclic loads are imaged using ultrasonic tomography before, during, and after loads are applied. Concrete columns with varying geometries and detailing, loading protocols, and material types are considered. The columns contain internally embedded concrete strain gauges, the data from which are used to establish extent of accumulated damage caused by the applied loads at certain locations within the columns. A newly developed hybrid air-coupled ultrasonic system is used to collect a large volume of through-thickness ultrasonic data across the cross section at the plastic hinge region of the column. Ultrasonic monitoring was carried out at increasing load levels up to a drift ratio of 1%. The ultrasonic data are used to back-calculate wave velocity tomographic images (tomograms) across the cross section. A comparison of ultrasonic and strain gauge data shows that ultrasonic tomograms indicate damage progression within the columns, considering both global and local spatial scales. The results also confirm that the UHP-FRC column exhibited much less internal damage at a given load level compared to conventional reinforced concrete columns.
Related References:
1. ASCE, “2013 Report Card for America’s Infrastructure,” www.infrastructurereportcard.org (accessed July 2016)
2. ACI Committee 546, “Concrete Repair Guide (ACI 546R-96),” American Concrete Institute, Farmington Hills, MI, 2001, 41 pp.
3. ACI Committee 374, “Acceptance Criteria for Moment Frames Based on Structural Testing (ACI 374.1-05) and Commentary,” American Concrete Institute, Farmington Hills, MI, 2005, 9 pp.
4. ACI Committee 228, “Report on Nondestructive Test Methods for Evaluation of Concrete Structure (ACI 228.2R-13),” American Concrete Institute, Farmington Hills, MI, 2013, 82 pp.
5. Maierhofer, C.; Reinhardt, H. W.; and Dobmann, G., “Non-Destructive Evaluation of Reinforced Concrete Structures” Non-Destructive Testing Methods, CRC Press, Boca Raton, FL, 2010.
6. Aggelis, D. G., “Wave Propagation through Engineering Materials; Assessment and Monitoring of Structures through Non-Destructive Techniques,” Materials and Structures, ASCE, V. 46, No. 4, 2013, pp. 519-532. doi: 10.1617/s11527-013-0020-x
7. Schickert, M.; Krause, M.; and Müller, W., “Ultrasonic Imaging of Concrete Elements Using Reconstruction by Synthetic Aperture Focusing Technique,” Journal of Materials in Civil Engineering, ASCE, V. 15, No. 3, 2003, pp. 235-246. doi: 10.1061/(ASCE)0899-1561(2003)15:3(235)
8. Shevaldykin, V.; Samakrutov, A.; and Kozlov, V., “Ultrasonic Low-Frequency Short Pulse Transducers with Dry Point Contact,” Development and Application, International Symposium Non-Destructive Testing in Civil Engineering (NDT-CE), Berlin, Germany, 2003, pp.16-19.
9. De La Haza, A. O.; Samokrutov, A. A.; and Samokrutov, P. A., “Assessment of Concrete Structures Using the Mira and Eyecon Ultrasonic Shear Wave Devices and the SAFT-C Image Reconstruction Technique,” Construction & Building Materials, V. 38, 2013, pp. 1276-1291. doi: 10.1016/j.conbuildmat.2011.06.002
10. Clayton, D.; Smith, C.; Ferraro, C.; Nelson, J.; Khazanovich, L.; Hoegh, K.; Chintakunta, S.; Popovics, J. S.; Choi, H.; and Ham, S., “Evaluation of Ultrasonic Techniques on Concrete Structures” Report: ORNL/TM-2013/430, Oak Ridge National Laboratory, Oak Ridge, TN, 2013.
11. Freeseman, K.; Khazanovich, L.; Hoegh, K.; Nojavan, A.; Schultz, A. E.; and Chao, S.-H., “Nondestructive Monitoring of Subsurface Damage Progression in Concrete Columns Damaged by Earthquake Loading,” Engineering Structures, V. 114, 2016, pp. 148-157. doi: 10.1016/j.engstruct.2016.02.017
12. Choi, H., and Popovics, J. S., “NDE Application of Ultrasonic Tomography to a Full-Scale Concrete Structure,” IEEE Transactions on Ultrasonics, Ferroelectrics, and Frequency Control, V. 62, No. 6, 2015, pp. 1076-1085. doi: 10.1109/TUFFC.2014.006962
13. Choi, H.; Bittner, J.; and Popovics, J. S., “Comparison of Ultrasonic Imaging Techniques for Full-Scale Reinforced Concrete,” Transportation Research Record: Journal of the Transportation Research Board, V. 2592, 2016, pp. 126-135. doi: 10.3141/2592-14
14. Choi, H.; Ham, Y.; and Popovics, J. S., “Integrated Visualization for Reinforced Concrete Using Ultrasonic Tomography and Image-Based 3-D Reconstruction,” Construction and Building Materials, V. 123, No. 1, 2016, pp. 384-393. doi: 10.1016/j.conbuildmat.2016.07.010
15. Aghdasi, P.; Heid, A. E.; and Chao, S.-H., “Developing Ultra-High-Performance Fiber-Reinforced Concrete For Large-Scale Structural Applications,” ACI Materials Journal, V. 113, No. 5, Sept.-Oct. 2016, pp. 559-570. doi: 10.14359/51689103
16. Palacios, G.; Liu, X.; Chao, S.-H.; Nojavan, A.; and Schultz, A. E., “Seismic Performance of a Highly Damage-Tolerant Ultra-High-Performance Fiber-Reinforced Concrete Column,” Paper No. 2833, 16th World Conference on Earthquake (16WCEE), Santiago Chile, 2017.
17. ACI Committee 318, “Building Code Requirements for Structural Concrete (318-11) and Commentary,” American Concrete Institute, Farmington Hills, MI, 2011, 473 pp.
18. Nojavan, A.; Schultz, A. E.; Haselton, C.; Simathathien, S.; Liu, X.; and Chao, S.-H., “A New Data Set for Full-Scale Reinforced Concrete Columns under Collapse-Consistent Loading Protocols,” Earthquake Spectra, V. 31, No. 2, 2015, pp. 1211-1231. doi: 10.1193/040314EQS047
19. Nojavan, A.; Schultz, A.; Liu, X.; Simasathien, S.; Palacios, G.; Chao, S.-H.; Haselton, C.; Choi, H.; and Popovics, J., “CI-1 RC Perimeter-Frame Column under Near Collapse Loading,” Network for Earthquake Engineering Simulation (distributor), Dataset, 2014. doi:10.4231/D3G44HQ9B.10.4231/D3G44HQ9B
20. Nojavan, A.; Schultz, A.; Liu, X.; Simasathien, S.; Palacios, G.; Chao, S.-H.; Haselton, C.; Choi, H.; and Popovics, J., “CI-7 RC Perimeter-Frame Column under Bi-Axial Loading Protocol,” Network for Earthquake Engineering Simulation (distributor), Dataset, 2014. doi:10.4231/D3BC3SX4Q.10.4231/D3BC3SX4Q
21. Nojavan, A.; Schultz, A.; Liu, X.; Simasathien, S.; Palacios, G.; Chao, S.-H.; Haselton, C.; Choi, H.; and Popovics, J., “CII-2 RC Space-Frame Column under Symmetric Cyclic Loading (ACI 374),” Network for Earthquake Engineering Simulation (distributor), Dataset, 2014. doi:10.4231/D3KW57J3S.10.4231/D3KW57J3S
22. Nojavan, A.; Schultz, A.; Liu, X.; Simasathien, S.; Palacios, G.; Chao, S.-H.; Haselton, C.; Choi, H.; and Popovics, J., “CIII-2 UHPFRC Space-Frame Column under Symmetric Cyclic Loading (ACI 374)”, Network for Earthquake Engineering Simulation (distributor), Dataset, 2014. doi:10.4231/D36M3340C.10.4231/D36M3340C
23. Cetragolo, G. P., and Popovics, J. S., “Inspection of Concrete Using Air-Coupled Ultrasonic Pulse Velocity,” ACI Materials Journal, V. 107, No. 2, Mar.-Apr. 2010, pp. 155-163.
24. King, D. A.; Malloy, M.; Roberts, A.; Haak, A.; Yoder, C.; and O’Brien, W. Jr., “Determination of Postexcitation Thresholds for Single Ultrasound Contrast Agent Microbubbles Using Double Passive Cavitation Detection,” Journal of the Acoustical Society of America, V. 127, No. 6, 2010, pp. 3449-3455. doi: 10.1121/1.3373405
25. Carpinteri, A.; Xu, J.; Lacidogna, G.; and Manuello, A., “Reliable Onset Time Determination and Source Location of Acoustic Emissions in Concrete Structures,” Cement and Concrete Composites, V. 34, No. 4, 2012, pp. 529-537. doi: 10.1016/j.cemconcomp.2011.11.013
26. Hu, B.; Kundu, T.; Grill, W.; Liu, B.; and Toufigh, V., “Embedded Piezoelectric Sensors for Health Monitoring of Concrete Structures,” ACI Materials Journal, V. 110, No. 2, Mar.-Apr. 2013, pp. 149-159.
27. Hansen, P. C., and Saxild-Hansen, M., “AIR Tools – A MATLAB Package of Algebraic Iterative Reconstruction Methods,” Journal of Computational and Applied Mathematics, V. 236, No. 8, 2012, pp. 2167-2178. doi: 10.1016/j.cam.2011.09.039
28. Choi, H., “Evaluation of Internal Damage in Reinforced Concrete Elements Using Ultrasonic Tomography,” PhD dissertation, University of Illinois at Urbana-Champaign, Champaign, IL, 2016.
29. Bousias, S.; Verzeletti, G.; Fardis, M.; and Gutierrez, E., “Load-Path Effects in Column Biaxial Bending with Axial Force,” Journal of Engineering Mechanics, ASCE, V. 121, No. 5, 1995, pp. 596-605. doi: 10.1061/(ASCE)0733-9399(1995)121:5(596)