Disc. 113-S103/From the November-December 2016 ACI Structural Journal

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Disc. 113-S103/From the November-December 2016 ACI Structural Journal

Author(s): Himat Solanki and Dharan Patel

Publication: Structural Journal

Volume: 114

Issue: 5

Appears on pages(s): 1363-1364

Keywords:

DOI:

Date: 9/1/2017

Abstract:
Disc. 113-S103/From the November-December 2016 ACI Structural Journal, p. 1209 Assessment of Shear Strength of Circular Reinforced Concrete Beams. Paper by Bijily Balakrishnan, Shehabaz Hussain, and Devdas Menon