Foamed Cement Generation Methods: Insights from Macro-Porosity and Void Distribution

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Foamed Cement Generation Methods: Insights from Macro-Porosity and Void Distribution

Author(s): L. E. Dalton, D. Crandall, K. Shanley, M. Gill, E. Rosenbaum, J. Moore, G. Ahmadi, B. Kutchko, and J. Chipkin

Publication: Materials Journal

Volume: 115

Issue: 1

Appears on pages(s): 89-103

Keywords: computed tomography scanning; foamed cement; wellbore cement; wellbore integrity

DOI: 10.14359/51701101

Date: 1/1/2018

Abstract:
The American Petroleum Institute (API) Recommended Practice 10B-4 is the industry standard for measuring foamed cement stability; however, it does not incorporate the effects of elevated pressure or placement. Using high-resolution computed tomography (CT) scanning, this study examines how cement slurry flow through pipes impacts void distribution in cured foamed cement. Analysis of void size and distribution allows a comparison of lab and field generation; simulated velocity profiles indicate cement flow through constrictions likely influences structural variations. Notably, field-generated samples show more nitrogen bubbles at the injection port. Moreover, a review of the average bubble diameter concludes lab samples have average bubble sizes that increase with their quality, while field samples have similar average bubble diameters suggesting variation among generation methods.

Related References:

1. Benge, G., and Poole, D., “Use of Foamed Cement in Deep Water Angola,” IADC/SPE Drilling Conference, Amsterdam, the Netherlands, Society of Petroleum Engineers, Feb. 2005, pp. 1-5.

2. Moore, S.; Miller, M.; and Faul, R., “Foam Cementing Applications of a Deepwater Subsalt Well—Case History,” IADC/SPE Drilling Conference, New Orleans, LA, Society of Petroleum Engineers, Feb. 23-25, 2000.

3. Taiwo, O., and Ogbonna, J., “Foam Cementing Design and Application: A Cure for Low Gradient-Associated Problems in Deepwater Operations in the Gulf of Guinea,” Nigeria Annual International Conference and Exhibition, Abuja, Nigeria, Africa, Society of Petroleum Engineers, July-Aug. 2011, pp. 1-7.

4. Kopp, K.; Redd, S.; Foreman, J.; Carty, B.; and Griffith, J., “Foamed Cement vs. Conventional Cement for Zonal Isolation—Case Histories,” Society of Petroleum Engineers, IADC/SPE Annual Technical Conference and Exhibition, Dallas, TX, Oct. 2000, pp. 1-9.

5. Griffith, J. E.; Lende, G.; Ravi, K.; Saasen, A.; Nødland, N. E.; and Jordal, O. H., “Foamed Cement Engineering and Implementation for Cement Sheath Integrity at High Temperature and High Pressure,” Society of Petroleum Engineers, IADC/SPE Drilling Conference, Dallas, TX, Mar. 2004, pp. 1-11.

6. Benge, O. G.; McDermott, J. R.; Langlinais, J. C.; and Griffith, J. E., “Foamed Cement Job Successful in Deep HTHP Offshore Well,” Oil & Gas Journal, V. 94, Mar. 1996, pp. 58-63.

7. Kutchko, B.; Pike, W.; Lang, K.; Strazisar, B.; and Rose, K., “An Assessment of Research Needs Related to Improving Primary Cement Isolation of Formations in Deep Offshore Wells, EPAct Technical Report Series,” U.S. Department of Energy, National Energy Technology Laboratory, Morgantown, WV, 2012, pp. 1-14.

8. Chief Counsel’s Report, “Macondo: The Gulf Oil Disaster,” National Commission on the BP Deepwater Horizon Oil Spill and Offshore Drilling, 2011, 371 pp.

9. API Recommended Practice 10B-4, “Preparation and Testing of Foamed Cement Slurries at Atmospheric Pressure,” second edition, American Petroleum Institute, Washington, DC, Oct. 2015, 48 pp.

10. Ley, T., and Tabb, B., “Development of a Robust Field Technique to Quantify the Air-Void Distribution in Fresh Concrete,” Oklahoma Transportation Center, Midwest City, OK, July 2013, 54 pp.

11. Kutchko, B.; Crandall, D.; Gill, M.; McIntyre, D.; Spaulding, R.; Strazisar, B.; Rosenbaum, E.; Haljasmaa, I.; Benge, G.; Cunningham, E.; DeBruijn, G.; and Gardner, C., “Computed Tomography and Statistical Analysis of Bubble Size Distributions in Atmospheric-Generated Foamed Cement,” Technical Report No. NETL-TRS-2-2013, EPAct Technical Report Series, U.S. Department of Energy, National Energy Technology Laboratory, Morgantown, WV, 2013, 32 pp.

12. Kutchko, B.; Crandall, D.; Moore, J.; Gill, M.; Haljasmaa, I.; Spaulding, R.; Harbert, W.; Benge, G.; DeBruijn, G.; and Shine, J., “Assessment of Pressurized Foamed Cement Used in Deep Offshore Wells,” SPE Deepwater Drilling and Completions Conference, Galveston, TX, Sept. 2014, 22 pp.

13. Kutchko, B.; Moore, J.; Crandall, D.; Gill, M.; McIntyre, D.; Spaulding, R.; Strazisar, B.; Rosenbaum, E.; Haljasmaa, I.; Benge, G.; Cunningham, E.; DeBruijn, G.; Shine, J.; and Gardner, C., “Addendum 1 to Computed Tomography and Statistical Analysis of Bubble Size Distributions in Atmospheric-Generated Foamed Cement,” NETL-TRS-2-2014, EPAct Technical Report Series, U.S. Department of Energy, National Energy Technology Laboratory, Morgantown, WV, Mar. 2014, 24 pp.

14. Kutchko, B.; Crandall, D.; Moore, J.; Gieger, C.; Gill, M.; Haljasmaa, I.; Spaulding, R.; Harbert, W.; Mergaman, A.; Dalton, L.; Rosenbaum, E.; McIntyre, D.; Benge, G.; Buford, C.; and Shine, J., “Assessment of Pressurized Foamed Cement Used in Deep Offshore Wells,” Offshore Technology Conference, Houston, TX, May 2015, 22 pp.

15. Kutchko, B.; Crandall, D.; Moore, J.; Gill, M.; McIntyre, D.; Rosenbaum, E.; Haljasmaa, I.; Strazisar, B.; Spaulding, R.; Harbert, W.; Benge, G.; DeBruijn, G.; Shine, J.; and Gardner, C., “Field-Generated Foamed Cement: Initial Collection, Computed Tomography, and Analysis,” Technical Report No. NETL-TRS-5-2015, EPAct Technical Report Series, U.S. Department of Energy, National Energy Technology, Morgantown, WV, July 2015, 52 pp.

16. Spaulding, R.; Haljasmaa, I.; Kutchko, B.; Fazio, J.; DeBruijn, G.; Shine, J. M.; Benge, G.; and Harbert, W., “An Assessment of the Dynamic Moduli of Atmospherically Generated Foam Cements,” Offshore Technology Conference, Houston, TX, May 2015, pp 1-17.

17. Benge, G., “Evaluation of the Cementing on the 9-7/8 x 7 Production String on the Macondo Well,” TREX-05990, Aug. 2011, 54 pp.

18. Al-Mashat, A. M., “Rheology of Foam Cement,” PhD dissertation, Colorado School of Mines, Golden, CO, 1977, 104 pp.

19. Harms, W. M., and Febus, J. S., “Cementing of Fragile-Formation Wells with Foamed Cement Slurries,” Journal of Petroleum Technology, V. 37, No. 6, 1985, pp. 1049-1057. doi: 10.2118/12755-PA

20. White, J.; Moore, S.; Miller, M.; and Faul, R., “Foaming Cement as a Deterrent to Compaction Damage in Deepwater Production,” Society of Petroleum Engineers, IADC/SPE Drilling Conference, New Orleans, LA, Feb. 2000, pp. 1-7.

21. de Rozieres, J., and Ferriere, R., “Foamed Cement Characterization under Downhole Conditions and Its Impact on Job Design,” Society of Petroleum Engineers Production Engineering, V. 6, No. 3, Aug. 1991, pp. 297-304.

22. Pang, X.; Singh, J. P.; Cuello Jimenez, W.; and Prince, A. C., “Influencing Factors of the Microstructure and Macroscopic Performance of Foamed Cement,” SPE Annual Technical Conference and Exhibition, Dubai, UAE, Sept. 26-28, 2016.

23. Jacobs, T., “Offshore Industry Gets a Fresh Look at Foamed Cement,” Journal of Petroleum Technology, V. 67, No. 1, 2015, pp. 58-63. doi: 10.2118/0115-0058-JPT

24. Rasband, W. S., and Image, J., U. S. National Institutes of Health, Bethesda, MD, 1997-2014, http://imagej.nih.gov/ij/. (last accessed Dec. 8, 2017)

25. “Avizo 8.0 User’s Guide,” Konrad-Zuse-Zentrum für Informationstechnik Berlin (ZIB), Germany, and Visualization Sciences Group, SAS, Germany, July 2013.

26. Meng, F.; Zhang, N.; and Wang, W., “Virtual Experimentation of Beam Hardening Effect in X-Ray CT Measurements of Multiphase Flow,” Elsevier Powder Technology, V. 194, No. 1-2, 2009, pp. 153-157. doi: 10.1016/j.powtec.2009.03.033

27. Cnudde, V., and Boone, M. N., “High-Resolution X-Ray Computed Tomography in Geosciences: A Review of the Current Technology and Applications,” Earth-Science Reviews, V. 123, 2013, pp. 1-17. doi: 10.1016/j.earscirev.2013.04.003

28. Weller, H.; Greenshields, C.; and Santos, B., “OpenFOAM,” The OpenFoam Foundation Ltd, London, UK, 2015.

29. Powers, T. C., The Properties of Fresh Cement, John Wiley & Sons Inc., New York, 1969, 686 pp.

30. Pang, X.; Maxson, J. K.; Cuello Jimenez, W.; Singh, J. P.; and Morgan, R. G., “Microscale Characterization of Field and Laboratory Foamed Cement Using X-Ray Micro Computed Tomography,” SPE Journal, V. 22, No. 5, 2017, 14 pp.


ALSO AVAILABLE IN:

Electronic Materials Journal