Optimization Performance of High Volume Fly Ash Self-Consolidating Mixtures with Hydrated Lime (Mortar Component)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Optimization Performance of High Volume Fly Ash Self-Consolidating Mixtures with Hydrated Lime (Mortar Component)

Author(s): Hayder Alghazali, John J. Myers

Publication: Symposium Paper

Volume: 320

Issue:

Appears on pages(s): 46.1-46.12

Keywords: sustainability, fly ash, hydrated lime, HVFA-SCC, performance ranking analysis approach

DOI: 10.14359/51701084

Date: 8/1/2017

Abstract:
As is known, more sustainable concrete has become the desired aim of many transportation departments. To produce more sustainable concrete, the emphasis has been placed on replacing cement with more sustainable materials and taken into account, materials cost and CO2 footprint. High volume fly ash with hydrated lime mixtures have been proposed as one potential approach for achieving durable and sustainable concrete. In this first phase study, performance ranking analysis approach is presented to optimize the performance of high volume fly ash mortars. A total of 15 mortar mixtures were prepared at different replacement levels (up to 75 percent). Hydrated lime was incorporated with ASTM Class C fly ash to increase hydration reaction at different dosage levels (between 0-15 percentages). Fresh properties and semi Adiabatic temperature tests were conducted for each mixture. Compressive strength, drying shrinkage, bulk electric conductivity, and electric resistivity (surface) were measured and monitored until the age of 90 days. Cost efficiency was also evaluated. Based on performance ranking approach, five different binder compositions were selected to conduct the second phase of this study.

Related References:

1. Benhelal, E., Zahedi, G., Shamsaei, E., and Bahadori, A., "Global strategies and potentials to curb CO2emissions in cement industry", Journal of Cleaner Production, 2013, V. 51: pp. 142-161.

2. Rubenstein, M., "Emissions from the cement industry". The Earth Institute of Columbia University, 2012.

3. Kosmatka, S.H., Wilson, M.L., "Design and control of concrete mixtures". 16th edition, 2016.

4. ACI Committee 232, "Use of Fly Ash in Concrete (ACI 232.2R-03)", American Concrete Institute, FarmingtonHills, MI, 2003.

5. Richardson, D.N., Beckemeier, K.W., and Volz, J.S., "Effects of Powder Additive on High-Volume Fly AshMixtures", ACI Materials Journal, August 2015, V. 112(4), pp. 535-546.

6. Fantilli, A.P. and Chiaia, B., "Eco-mechanical performances of cement-based materials: An application to selfconsolidatingconcrete", Construction and Building Materials, 2013. V. 40: pp. 189-196.

7. Malhotra, V. M. "High-performance high-volume fly ash concrete." ACI Materials Journal V. 24.7 (2002): pp.30-34.

8. Malhotra, V. M. "High-performance HVFA concrete: A solution to the infrastructural needs of India." IndianConcrete Journal, V. 76.2 (2002): pp. 103-107.

9. Bouzoubaa, N., Zhang, M.H. and Malhotra, V.M. “Mechanical properties and durability of concrete made withhigh-volume fly ash blended cements using a coarse fly ash.” Cement and Concrete Research, 2001, V.31(10), pp.1393-1402.

10. Vaughn, N. and Polnaszek, C., "Design-Expert® software", version 10, Stat-Ease, Inc, Minneapolis, MN, 2010.

11. ASTM (2015) " Standard test method for flow of hydraulic cement mortar.", ASTM C1437, WestConshohocken, PA.

12. ASTM (2015) "Standard Test Method for Compressive Strength of Hydraulic Cement Mortars (Using 2-in. or

50-mm. Cube Specimens).", ASTM C109, West Conshohocken, PA.

13. ASTM (2004) "Standard Test Method for Drying Shrinkage of Mortar Containing Hydraulic Cement.", ASTMC596, West Conshohocken, PA.

14. AASHTO (2011) “Standard Method of Test for Surface Resistivity Indication of Concrete’s Ability to Resist Chloride Ion Penetration.” T95, Washington, DC.

15. ASTM (2012) " Standard Test Method for Bulk Electrical Conductivity of Hardened Concrete.", ASTMC1760, West Conshohocken, PA.

16. Islam, M.M. and Islam, M.S., "Strength behavior of mortar using fly ash as partial replacement of cement".Concrete Research Letters, 2010, V. 1(3), pp. 98-106.

17. Holland, N., Nichols, A., and Nichols, J., "The Use of Hydrated Lime in Concrete as a Cement Replacement:Effect on Compressive Strength", Lime: Building on the 100-Year Legacy of The ASTM Committee C07.2012, ASTM International.

18. Ghafari, E., Costa, H., Júlio, E., "Statistical mixture design approach for eco-efficient UHPC", Cement &Concrete Composites, V. 55, January 2015, pp. 17-25.

19. Khayat, K.H., Yahia, A., Sayed, M., "Effect of Supplementary Cementitious Materials on rheologicalProperties, Bleeding, and Strength of Structural Grout", ACI Materials Journal, V. 105 (6), 2008, pp.585-593.