Development of Test Methods and Specifications for Chemically Activated Binders

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Development of Test Methods and Specifications for Chemically Activated Binders

Author(s): R. Douglas Hooton, Lawrence Sutter, and Mary Christiansen

Publication: Symposium Paper

Volume: 320

Issue:

Appears on pages(s): 38.1-38.12

Keywords: alternative cements; building codes; chemically activated binders; durability tests; test methods.

DOI: 10.14359/51701076

Date: 8/1/2017

Abstract:
There has been a proliferation of research and development activity focused on chemically activated binder technologies and other alternative cements for use in concrete. Some activated binder technologies have been used successfully in construction or in manufacture of building products. However, a major barrier to adoption of such new materials is the lack of appropriate test methods and specifications, often precluding their use in structural applications since they are not covered by building codes. Some existing test methods may be suspect for evaluation of new cementing materials because they often do not relate well to field performance for portland cement concrete. However, engineers have experience, familiarity and a comfort level with using portland cement concrete. In addition to raising specific areas of concern with existing test methods, alternative approaches to adapting existing test methods or development of new tests specific to evaluation of chemically activated binders and alternative cements are discussed.