Title: Properties of Self-Compacting Concrete with Natural and Synthetic Fibers

Author(s): Tahar Tioua, Abdelouahed Kriker, Abderrahim Bali, Gonzalo Barluenga and Mourad Behim

Publication: Symposium Paper

Volume: 320

Issue:

Appears on pages(s): 24.1-24.10

Keywords: date palm fiber, flowability, hardened properties, polypropylene fiber, self-compacting concrete

DOI: 10.14359/51701062

Date: 8/1/2017

Abstract:
An experimental study was carried out to assess the effect of low volumetric fractions of short natural date palm fibers (DPF) compared to polypropylene fibers (PPF) on self-compacting concrete (SCC) flowability and hardened properties. Fibers can reduce concrete shrinkage cracking at early age and enhance other hardened concrete properties, although reducing other characteristics as SCC flowability. The use of DPF instead of PPF has two advantages: their use in construction provides new outlets for low cost agricultural resources, and the valorization of natural fibers allows to reduce environmental impacts, since these are renewable raw materials and need little energy to be produced. Slump flow, V-funnel and L box tests were used to assess flowability. Mechanical and physical properties, including compressive and flexural strength, were also measured. It was found that DPF can successfully replace PPF although DPF reduced SCC flowability slightly more than PPF, but produced similar effects in SCC hardened properties.

Related References:

1. Akram, T., Memon, S.A., Obaid, H., “Production of low cost self- compacting concrete using bagasse ash," Construction and Building Materials, V. 23, No. 2, 2009, pp. 703–712.

2. Rozière, E., Granger, S., Turcry, Ph., Loukili, A., “Influence of paste volume on shrinkage cracking and fracture properties of self-compacting concrete,? Cement and Concrete Composites, V. 29, No. 8, 2007, pp. 626–636.

3. Yadegaran I., Mahoutian M., Shekarchi N., “Effect of polypropylene fibers on shrinkage of self-compacting concrete," In: 5th International RILEM symposium on self compacting concrete. Ghent-Belgium: RILEM Publications, 2007, pp. 707–713.

4. El-Dieb, A.S., and Reda Taha, M.M., “Flow characteristics and acceptance criteria of fiber-reinforced selfcompacted concrete (FR-SCC)," Construction and Building Materials, V. 27, 2012, pp. 585–596.

5. Kriker, A., Debicki, G., Bali, A., Khenfer, M. M., Chabannet, M., “Mechanical properties of date palm fibers and concrete reinforced with date palm fibers in hot-dry climate," Cement Concrete Composites, V. 27, No. 5, 2005, pp. 554-564.

6. Sellami, A., Merzoud, M., Amziane, S., “Improvement of mechanical properties of green concrete by treatment of the vegetables fibers,? Construction and Building Materials, V. 47, 2013, pp. 1117–1124.

7. Barluenga, G., and Hernandez-Olivares, F., “Cracking control of concretes modified with short AR-glass fibers at early age: experimental results on standard concrete and SCC,? Cement and Concrete Research, V. 37, No. 12, 2007, pp. 1624–1638.

8. Sabry, A. A., “Properties and mesostructural characteristics of linen fiber reinforced self-compacting concrete in slender columns," Ain Shams Engineering Journal, V. 4, 2013, pp. 155–161.

9. Saeid, H., Iman S. H., Seyed A. A. E., “Mechanical behavior of self-compacting concrete pavements incorporating recycled tire rubber crumb and reinforced with polypropylene fiber,? Journal of Cleaner Production, V. 133, 2016, pp. 228-234.

10. Mohamed, M.A.S., Ghorbel, E., Wardeh, G., “Valorization of micro-cellulose fibers in self-compacting concrete," Construction and Building Materials, V. 24, 2010, pp. 2473–2480.

11. Balaguru, P.N. and Shah S.P., “Plastic and early drying shrinkage,? Chapter 11 in Fiber Reinforced Cement Composites, McGraw-Hill, 1992.

12. Flores Medina, N., Barluenga, G., Hernandez-Olivares, F., “Enhancement of durability of concrete composites containing natural pozzolans blended cement through the use of Polypropylene fibers," Composites: Part B, V. 61, 2014, pp. 214-221.

13. Sun, Z. and Xu, Q., “Microscopic, physical and mechanical analysis of polypropylene fiber reinforced concrete," Materials Science and Engineering A, V. 527, No. 1-2, 2009, pp. 198-204.