Effects of Ternary Cements with Limestone Filler on DEF in Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effects of Ternary Cements with Limestone Filler on DEF in Concrete

Author(s): Yasser Amine, Nordine Leklou, Ouali Amiri

Publication: Symposium Paper

Volume: 320

Issue:

Appears on pages(s): 20.1-20.14

Keywords: concrete, delayed ettringite formation, expansion, heat curing, limestone filler, mineral admixtures, ternary blend

DOI: 10.14359/51701058

Date: 8/1/2017

Abstract:
In this study, the effect of limestone filler in addition to other mineral admixtures on the expansion of concrete caused by internal sulfate attack was investigated. For this purpose, three different admixtures (fly ash, metakaolin and natural pozzolan) were incorporated in heat-cured concretes for a total cement replacement ratio of 25%. Tests of length changes, compressive strength, dynamic modulus of elasticity, and apparent porosity were carried out on these concretes over a period of 650 days. Additionally, microcalorimetry tests on cement pastes with w/cm ratio equal to 0.35 were conducted. Furthermore, thermogravimetric analysis was conducted to identify the phases formed due to the limestone filler. The results obtained were analyzed and highlighted the correlation between the microstructural and mechanical properties of the heat-cured concretes and their expansion. The important role of limestone filler in ternary formulations and the inhibitory effect of admixtures (fly ash and metakaolin) on DEF was also highlighted.

Related References:

1. Pavoine, A. 2003. “Evaluation du potentiel de réactivité des bétons vis-à-vis de la formation différée de l'ettringite”,Doctoral dissertation Paris 6.

2. Taylor, H.F.W., Famy, C., and Scrivener, K.L. 2001. “Delayed ettringite formation”, Cement and concrete research, Vol.31, No. 5, pp. 683-693.

3. Zhang, Z., Olek, J., and Diamond, S. 2002. “Studies on delayed ettringite formation in early-age, heat-cured mortars: I.Expansion measurements, changes in dynamic modulus of elasticity, and weight gains”, Cement and concrete Research, Vol.32, No. 11, pp. 1729-1736.

4. Nguyen V.H. 2013. “Effet d’addition minérale sur l’apparition de la Réaction Sulfatique interne : étude paramétrique,développement et optimisation de méthodes accélérés”, Doctoral dissertation, University of Nantes, 2013.

5. Ramlochan T., Zacarias P., Thomas M.D.A., and Hooton R.D. 2003. “The effect of pozzolans and slag on the expansionof mortars cured at elevated temperature, Part I: Expansive behaviour”, Cement and Concrete Research, , Vol. 34, No. 08, pp.1341-1356.

6. Nguyen V.H., Leklou N., Aubert, J.E, and Mounanga P. 2013. “The effect of natural pozzolan on delayed ettringiteformation of the heat-cured mortars”, Construction and Building Materials, Vol. 48, pp. 479-484.

7. Leklou, N., Nguyen, V. H., and Mounanga, P. 2017. “The effect of the partial cement substitution with fly ash on delayedettringite formation in heat-cured mortars”, KSCE Journal of Civil Engineering, Vol. 21, No. 4, pp 1359–1366.

8. Opoczky, L. 1992. “Progress of the particle size distribution during the intergrading of a clinker-limestone mixture”, Zem-Kalk-Gips, Vol. 45, pp. 648-651.

9. Poppe, A.M. and De Schutter, G. 2005. “Cement hydration in the presence of high filler contents.”, Cement and ConcreteResearch, Vol. 35, No. 12, pp.2290-2299.

10. Moon, G.D., Oh, S., Jung, S.H., and Choi, Y.C. 2017. “Effects of the fineness of limestone powder and cement on thehydration and strength development of PLC concrete”, Construction and Building Materials, Vol.135, pp. 129-136.

11. Ye, G., Liu, X., De Schutter, G., Poppe, A.M. and Taerwe, L. 2007. “Influence of limestone powder used as filler in SCCon hydration and microstructure of cement pastes”, Cement and Concrete Composites, Vol. 29, No. 02, pp. 94-102.

12. Poppe, A.M. 2004. “Influence of fillers on hydration and properties of self-compacting concrete”, Doctoral dissertation,Magnel Laboratory for Concrete Research, Ghent University.

13. Silva, A.S., Soares, D., Matos, L., Salta, M., Divet, L., Pavoine, A., Candeias, A., and Mirão, J. 2010. “Influence ofMineral Additions in the Inhibition of Delayed Ettringite Formation in Cement based Materials–A MicrostructuralCharacterization”, Materials Science Forum, Vol. 636-637, pp. 1272-1279.

14. Kurdowski, W., and Duszak, S. 2002. “Can addition of limestone eliminate the expansion of the mortars due to DEF?”,International RILEM Workshop on International Sulfate Attack and Delayed Ettringite Formation. Vol. 35, RILEMPublications.

15. Al Shamaa, M., Lavaud, S., Divet, L., Colliat, J.B., Nahas, G. and Torrenti, J.M. 2016. “Influence of limestone filler andof the size of the aggregates on DEF”, Cement and Concrete Composites Vol.71, pp. 175-180.

16. Arliguie, G., and Hornain, H. 2007. “GranDuBé : Grandeurs associées à la Durabilité des Bétons”, Presse des Ponts.

17. Stark, J., and Bollmann, K. 2000 “Delayed ettringite formation in concrete”, Nordic Concrete Research-Publications,Vol. 23, pp. 4-28.

18. Divet, L. 2001. “Les réactions sulfatiques internes au béton : contribution à l’étude des mécanismes de la formationdifférée de l’ettringite”, Doctoral dissertation, Conservatoire National des Arts et Métiers de Paris.

19. Martin, R.P. 2010. “Analyse sur structures modèles des effets mécaniques de la Réaction Sulfatique Interne du béton”,Doctoral dissertation, University Paris Est.

20. Brunetaud, X., Divet, L., and Damidot, D. 2008. “Impact of unrestrained delayed ettringite formation induced expansionon concrete mechanical properties”, Cement and Concrete Research, Vol. 38, No. 11, pp. 1343–1348.

21. AFREM, AFGC. 1997. “Méthodes recommandées pour la mesure des grandeurs associées à la durabilité”, Compte rendudes journées techniques AFPC-AFREM, Durabilité des bétons.

22. Frias, M., De Rojas, M.S., and Cabrera, J. 2002. “The effect that the pozzolanic reaction of metakaolin has on the heatevolution in metakaolin-cement mortars”, Cement and Concrete Research, Vol. 30, No. 02, pp. 209-216.

23. Langan, B.W., Weng, K., and Ward. M.A. 2002. “Effect of silica fume and fly ash on heat of hydration of Portlandcement”, Cement and Concrete Research, Vol. 32, No. 07, pp. 1045-1051.

24. AFNOR Normalisation NF P 18-585. 1990. “Granulats–Stabilité dimensionnelle en milieu alcalin-Essai sur mortier.Expérimentale”.

25. Kretz, T., Godart, B. and Divet, L. 2009. “Recommendations for preventing disorders due to delayed ettringiteformation”, Guide technique of the laboratoires des ponts et chaussées.

26. Brunetaud., X. 2005. “Etude de l’influence de différents paramètres et de leurs interactions sur la cinétique et l’amplitudede la réaction sulfatique interne au béton”, Doctoral dissertation, Ecole Centrale des Arts et Manufactures de Paris.

27. Leklou, N., Aubert, J.E., and Escadeillas, G. 2009. “Microscopic observations of samples affected by delayed ettringiteformation (DEF)”, Materials and structures, Vol.42, No. 10, pp. 1369-1378.

28. Petrov, N., and Tagnit-Hamou A. 2004. “Is microcracking really precursor to DEF and consequent expansion?”, ACIMaterials Journal, Vol. 101, No. 6, pp. 442-447.

29. Wild, S., and Khatib, J.M. 1997. “Portlandite consumption in metakaolin cement pastes and mortars”, Cement andConcrete Research Vol. 27, No. 1, pp. 137-146.

30. Baroghel-Bouny, V. 1994. “Caractérisation des pâtes de ciment et des bétons-Méthodes, analyses, interprétations”,Journal du LCPC, pp. 92-93.

31. Aqel, M., and Panesar, D.K. 2016. “Hydration kinetics and compressive strength of steam-cured cement pastes andmortars containing limestone filler”, Construction and Building Materials Vol. 113, pp. 359-368.

32. Ollivier, J.P., and Baron, J. 1997. “Les bétons : Bases et données pour leur formulation”, Paris : Eyrolles. Chicago.

33. Kuzel, H.J., and Pöllmann, H. 1993. “Hydration of C3A in the presence of Ca(OH)2, CaSO4.2H2O and CaCO3”, CementConcrete Research, Vol.21, No. 5, pp. 885-895.

34. Chloup-Bondant, M. 1996. “Etude des mécanismes réactionnels dans l'hydratation des silicates et aluminates tricalciquesen présence d'un filler calcaire”, Doctoral dissertation, Nancy 1.

35. Kuzel, H.J., and Meyer, H. 1993. “Mechanisms of ettringite and monosulfate formation in cement and concrete in thepresence of CO3-2”, Proceedings of the 15th international conference on cement microscopy, Dallas.

36. Zajac, M., Rossberg, A., Le Saout, G., and Lothenbach, B. 2014. “Influence of limestone and anhydrite on the hydrationof Portland cements”, Cement and Concrete Composites, Vol. 46, pp. 99-108.