Influence of Pozzolanic Materials on the Hydration of Calcium Sulfoaluminate Cements

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Influence of Pozzolanic Materials on the Hydration of Calcium Sulfoaluminate Cements

Author(s): Frank Winnefeld, Lukas H.J. Martin, Elsa Tschopp, Christian J. Müller and Barbara Lothenbach

Publication: Symposium Paper

Volume: 320

Issue:

Appears on pages(s): 15.1-15.12

Keywords: Calcium sulfoaluminate cement, alternative binders, supplementary cementitious materials, pozzolan, fly ash, silica fume, thermodynamic modelling

DOI: 10.14359/51701053

Date: 8/1/2017

Abstract:
Calcium sulfoaluminate (CSA) cements are receiving increasing interest because they promise to provide a low–CO2 alternative to portland cement. In order to save costs and to further reduce the amount of CO2 attributed to the production of CSA, they are often blended with supplementary cementitious materials (SCMs) such as limestone powder or industrial by-products such as slag or fly ash. In portland cement systems, pozzolanic SCMs react with portlandite to form C-S-H. In CSA cements this reaction path is not possible as portlandite is generally not present in the hydrate assemblage. In this contribution, thermodynamic modelling is used to assess how pozzolanic SCMs may contribute to the hydration reactions and change the hydrate assemblage of CSA cements. The calculated hydrate compositions are compared to experimental data proving that pozzolanic SCMs are able to contribute to the hydration reactions of CSA cements.

Related References:

1. Gartner, E., 2004, “Industrially interesting approaches to "low-CO2" cements”, Cement and ConcreteResearch, 34, 1489-1498.

2. Juenger, M.C.G., Winnefeld, F., Provis, J.L., and Ideker, J.H., 2011, “Advances in alternative cementitiousbinders”, Cement and Concrete Research, 41, 1232-1243.

3. Glasser, F.P., and Zhang, L., 2001, “High-performance cement matrices based on calcium sulfoaluminatebelitecompositions”, Cement and Concrete Research, 21, 1881-1886.

4. Majling, J., Znasik, R., Gabrisova, A., and Svetik, S., 1985, “The influence of anhydrite activity upon thehydration of calcium sulfoaluminate cement clinker”, Thermochimica Acta, 92, 349-352.

5. Winnefeld, F., and Barlag, S., 2010, “Calorimetric and thermogravimetric study on the influence of calciumsulfate on the hydration of ye'elimite”, Journal of Thermal Analysis and Calorimetry, 101, 949-957.

6. Winnefeld, F., and Lothenbach, B., 2010, “Hydration of calcium sulfoaluminate cements - Experimentalfindings and thermodynamic modelling”, Cement and Concrete Research, 40, 1239-1247.

7. García-Maté, M., De la Torre, A.G., León-Reina, L., Losilla, E.R., Aranda, M.A.G., and Santacruz, I., 2015,“Effect of calcium sulfate source on the hydration of calcium sulfoaluminate eco-cement”, Cement and ConcreteComposites, 55, 53-61.sulphoaluminate clinker with additions of different calcium sulphate sources”, Materials and Structures, 49,453-466.

9. Winnefeld, F., and Lothenbach, B., 2016, “Phase equilibria in the system Ca4Al6O12SO4 – Ca2SiO4 – CaSO4– H2O referring to the hydration of calcium sulfoaluminate cements”, RILEM Technical Letters, 1, 10-16.

10. Zivica, V., 2000, “Properties of blended sulfoaluminate belite cement”, Construction and BuildingMaterials, 14, 433-437.

11. Pelletier-Chaignat, L., Winnefeld, F., Lothenbach, B., and Müller, C.M., 2012, Beneficial use of limestonefiller with calcium sulphoaluminate cement”, Construction and Building Materials, 26, 619-627.

12. Garcia-Mate, M., de la Torre, A.G., Leon-Reina, L., Aranda, M.A.G, and Santacruz, I., 2013, “Hydrationstudies of calcium sulfoaluminate cements blended with fly ash”, Cement and Concrete Research, 4, 12-20.

13. Ioannou, S., Reig, L., Paine, K., and Quillin, K., 2014, “Properties of a ternary calcium sulfoaluminatecalciumsulfate-fly ash cement”, Cement and Concrete Research, 56, 75-83.

14. Ma, B., Li, X.R., Shen, X.D., Mao, Y.Y., and Huang, H., 2014, “Enhancing the addition of fly ash fromthermal power plants in activated high belite sulfoaluminate cement”, Construction and Building Materials, 52,261-266.

15. Hargis, G.W., Telesca, A., and Monteiro, P.J.M., 2014, “Calcium sulfoaluminate (ye’elemite) hydration inthe presence of gypsum, calcite and vaterite”, Cement and Concrete Research, 65, 15-20.

16. Martin, L.H.J., Winnefeld, F., Müller, C., and Lothenbach, B., 2015, “Contribution of limestone to thehydration of calcium sulfoaluminate cement”, Cement and Concrete Composites, 62, 204-211.

17. Winnefeld, F., Tomasulo, M., Marroccoli, M., and Telesca, A., 2015, “Influence of microsilica on thehydration of ye’elimite”, 14th International Congress on the Chemistry of Cement, Beijing, China, Oct. 13-16,2015, 9 pp.

18. Martin, L.H.J., Lothenbach, B., Tschopp, E., Müller, C. J., and Winnefeld, F., 2015, “Blending calciumsulfoaluminate cement with fly ash”. 14th International Congress on the Chemistry of Cement, Beijing, China,Oct. 13-16, 2015, 8 pp.

19. Martin, L.H.J., Lothenbach, B., Tschopp, E., Müller, C., and Winnefeld, F., 2017, “Influence of fly ash onthe hydration of calcium sulfoaluminate cement”, Cement and Concrete Research, 95, 152-163.

20. Lothenbach, B., Scrivener, K., and Hooton, R.D., 2011, “Supplementary cementitious materials”, Cementand Concrete Research, 41, 1244-1256.

21. Wadsö, L., 2005, “Applications of an eight-channel isothermal conduction calorimeter for cementhydration studies”, Cement International, 5, 94-101.

22. Lumley, J.S., Gollop, R.S., Moir, G.K., and Taylor, H.F.W., 1996, “Degrees of reaction of the slag in someblends with Portland cements”, Cement and Concrete Research, 26, 139-151.

23. Ben Haha, M., De Weerdt, K., and Lothenbach, B., 2010, “Quantification of the degree of reaction of flyash”, Cement and Concrete Research, 40, 1620-1629.

24. Kulik, D.A., Wagner, T., Dmytrieva, S.V., Kosakowski, G., Hingerl, F.F., Chudnenko, K.V., and Berner,U., 2013, “GEM-Selektor geochemical modeling package: revised algorithm and GEMS3K numerical kernel forcoupled simulation codes”, Computational Geosciences, 17, 2013, 1-24.

25. Wagner, T., Kulik, D.A., Hingerl, F.F., and Dmytrieva, S.V., 2012, “GEM-Selektor geochemical modelingpackage: TSolMod library and data interface for multicomponent phase models”, Canadian Mineralogist, 50,1173-1195.

26. Hummel, W., Berner, U., Curti, E., Pearson, F.J., and Thoenen, T., 2002, “Nagra/PSI ChemicalThermodynamic Data Base 01/01”, Universal Publishers/uPUBLISH.com, USA, also published as NagraTechnical Report NTB 02-16, Wettingen, Switzerland.

27. Matschei, T., Lothenbach, B., and Glasser, F., 2007, “Thermodynamic properties of Portland cementhydrates in the system CaO-Al2O3-SiO2-CaSO4-CaCO3-H2O”, Cement and Concrete Research, 37, 1379-1410.

28. Lothenbach, B., Matschei, T., Möschner, G., and Glasser, F.P., 2008, “Thermodynamic modelling of theeffect of temperature on the hydration and porosity of Portland cement”, Cement and Concrete Research, 38, 1-18.

29. Lothenbach, B., Pelletier-Chaignat, L., Winnefeld, F., 2012, “Stability in the system CaO-Al2O3-H2O”,Cement and Concrete Research, 42, 1621-1634.