Title: 423.3R-17: Recommendations for Concrete Members Prestressed with Single-Strand Unbonded Tendons

Author(s): ACI Committee 423

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 24

Keywords: concrete slabs; cracking; fire resistance; joints; punching shear; unbonded post-tensioning

DOI:

Date: 9/7/2017

Abstract:
This report provides information for the design of flexural concrete members in buildings post-tensioned with single-strand unbonded tendons. The report is intended to complement the commentary in ACI 318 and to provide suggestions for revisions and additions to ACI 318. Consideration is given to design for gravity and lateral loads, determination of fire endurance, design for seismic forces, and design for catastrophic loadings. Recommendations concerning details and properties of tendons, protection against corrosion, and construction procedures are presented.