Influence of Permeability-Reducing Admixtures on Water Penetration in Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Influence of Permeability-Reducing Admixtures on Water Penetration in Concrete

Author(s): Mohammadreza Hassani E., Kirk Vessalas, Vute Sirivivatnanon, and Daksh Baweja

Publication: Materials Journal

Volume: 114

Issue: 6

Appears on pages(s): 911-922

Keywords: absorption; ANOVA; chemical admixture; permeability; permeability-reducing admixture; water penetration

DOI: 10.14359/51701002

Date: 11/1/2017

Abstract:
An experimental investigation was carried out on concrete into the effectiveness of integral permeability-reducing admixtures as possible alternatives to the traditional external waterproofers. The efficiency of hydrophobic water repellents and crystalline pore blockers were evaluated in concretes incorporating fixed water-cementitious materials ratio (w/cm) and different cementitious material types covering OPC, fly ash, and granulated blast-furnace slag. Three different test methods were employed to evaluate the water penetration resistance of concrete. To isolate the benefits that are achieved by varying the mixture design parameters, statistical factorial analysis of variances was carried out to discover the significance of each variable. Results indicated that the effect of w/cm and cementitious material is more pronounced compared to the addition of permeability-reducing admixtures. It was also demonstrated that the admixtures can be effective in reducing water penetration; however, their effect is varied in different mixtures. Caution must be exercised when using such admixtures in different concrete mixtures.

Related References:

1. The Concrete Society, “The Influence of Integral Permeability-Reducing Admixtures on the Durability of Concrete,” The Concrete Society, London, UK, 2013, pp. 5-6.

2. ACI Committee 212, “Report on Chemical Admixtures for Concrete (ACI 212.3R-16),” American Concrete Institute, Farmington Hills, MI, 2016, pp. 43-48.

3. Day, K. W.; Aldred, J.; and Hudson, B., Concrete Mix Design, Quality Control and Specification, fourth edition, CRC Press, Boca Raton, FL, 2013, pp. 65-86.

4. Rixom, M. R., and Mailvaganam, N. P., Chemical Admixtures for Concrete, E&FN Spon, London, UK, 1999, pp. 165-177.

5. Dao, V. T. N.; Dux, P. F.; Morris, P. H.; and Carse, A. H., “Performance of Permeability-Reducing Admixtures in Marine Concrete Structures,” ACI Materials Journal, V. 107, No. 3, May-June 2010, pp. 291-296.

6. Justnes, H., “Low Water Permeability through Hydrophobicity,” COIN Project Report 1, SINTEF Building and Infrastructure, Oslo, Norway, 2008, 36 pp.

7. Trinder, P. W., and Chalmers, C., “Resistance for Concrete to Harsh Environment—Ammonium Sulphate,” Concrete in Australia, 1999, 16 pp.

8. Yodmalai, D., and Sahamitmongkol, R., “Chloride Resistance of Cement Paste with Crystalline Materials,” Annual Concrete Conference 6, Thailand, 2010, pp. 365-370.

9. Aldred, J. M.; Swaddiwudhipong, S.; Lee, S. L.; and Wee, T. H., “The Effect of Initial Moisture Content on Water Transport in Concrete Containing a Hydrophobic Admixture,” Magazine of Concrete Research, V. 53, No. 2, 2001, pp. 127-134. doi: 10.1680/macr.2001.53.2.127

10. Roberts, M. H., and Adderson, B. W., “Tests on Permeability-Reducing Admixtures for Concrete,” B.R.E Technical Note No. 159/85, 1985, 66 pp.

11. Turl, S., “Concrete Waterproofers—Types, Mechanisms and Effectiveness,” Imperial College, Final Year Project, London, UK, 2011, 112 pp.

12. AS 1478.1-2000, “Chemical Admixtures for Concrete, Mortar and Grout—Admixtures for Concrete,” Standards Australia, Sydney, NSW, Australia, 2000, 47 pp.

13. AS 3972-2010, “General Purpose and Blended Cements,” Standards Australia, Sydney, NSW, Australia, 2010, 19 pp.

14. AS 3582.1-1998, “Supplementary Cementitious Materials for Use with Portland and Blended Cement—Fly Ash,” Standards Australia, Sydney, NSW, Australia, 1998, 9 pp.

15. AS 3582.2-2001, “Supplementary Cementitious Materials for Use with Portland and Blended Cement—Slag – Ground Granulated Iron Blast-Furnace,” Standards Australia, Sydney, NSW, Australia, 2001, 9 pp.

16. AS 2758.1-2014, “Aggregates and Rock for Engineering Purposes—Part 1: Concrete Aggregates,” Standards Australia, Sydney, NSW, Australia, 2014, 24 pp.

17. Hewlett, P. C., Lea’s Chemistry of Cement and Concrete, fourth edition, John Wiley & Sons, Inc., New York, 1998, pp. 837-896.

18. Bohren, C. F., and Huffman, D. R., Absorption and Scattering of Light by Small Particles, John Wiley & Sons, Inc., New York, 2008, 530 pp.

19. ASTM C642-13, “Standard Test Method for Density, Absorption, and Voids in Hardened Concrete,” ASTM International, West Conshohocken, PA, 2013, 3 pp.

20. AS 1012.8.1-2014, “Methods of Testing Concrete Method 8.1: Method for Making and Curing Concrete,” Standards Australia, Sydney, NSW, Australia, 2014, 10 pp.

21. BS EN 12390-8-2009, “Testing Hardened Concrete, Part 8: Depth of Penetration of Water under Pressure,” British Standards Institution, London, UK, 2009, 22 pp.

22. Khatri, R. P., and Sirivivatnanon, V., “Methods for the Determination of Water Permeability of Concrete,” ACI Materials Journal, V. 94, No. 3, May-June 1997, pp. 257-261.

23. AS 1012.9-2014, “Methods of Testing Concrete—Compressive Strength Tests – Concrete, Mortar and Grout Specimens,” Standards Australia, Sydney, NSW, Australia, 2014, 11 pp.

24. Basheer, P. A. M.; Montgomery, F. R.; and Long, A. E., “Factorial Experimental Design for Concrete Durability Research,” Proceedings of the Institution of Civil Engineers. Structures and Buildings, V. 104, No. 4, 1994, pp. 449-462. doi: 10.1680/istbu.1994.27203

25. Box, G. E. P.; Hunter, J. S.; and Hunter, W. G., Statistics for Experimenters—Design, Innovation, and Discovery, second edition, John Wiley & Sons, Inc., New York, 2005, pp. 173-234.


ALSO AVAILABLE IN:

Electronic Materials Journal